Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.59 MPa
230 psi
200%, post cured- 4 hours at 204°C
Multibase SILASTIC® C7-4535 VAROX Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.59 MPa
230 psi
TM R050-36
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Tensile Strength, Yield 1.59 MPa
230 psi
at 200%, molded-without post cure; ASTM D412
Multibase C6-235 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.59 MPa
230 psi
100%; ASTM D412
Teknor Apex Flexalloy® 3500-35 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
Tensile Strength, Yield 1.59 MPa
230 psi
ASTM D638
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in ..
Tensile Strength, Yield 1.59 MPa

@Strain 300 %
230 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 36-018 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerGood Surface AppearanceOpaqueApplications:AutomotiveInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by P..
Tensile Strength, Yield 1.59 - 52.0 MPa
230 - 7540 psi
Average value: 14.2 MPa Grade Count:143
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Tensile Strength, Yield 1.59 MPa

@Strain 300 %
230 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3830MS Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tensile Strength, Yield 1.59 MPa

@Strain 300 %
230 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3830MS Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tensile Strength, Yield 1.59 MPa

@Strain 300 %
230 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® ST-6130 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTransparentOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne ..