Material Notes:
Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
Instant; ASTM D2240
Tensile Strength, Yield 5.38 MPa
780 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.28 MPa

@Strain 300 %
330 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 700 %
700 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 21.9 kN/m
125 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 21 %
21 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified