Polymer Property : Linear Mold Shrinkage = 0.026 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KE2095-50AB Elastomer
KE-2095-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KEG2000-60A/B Elastomer
KEG2000-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KEG2000-70A/B Elastomer
KEG2000-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KEG2001-50A/B Elastomer
KEG2001-50 is a very fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enou..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KEG2002-50A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
ASTM D955
Teknor Apex Monprene® MP-2290A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KE2095-60AB Elastomer
KE-2095-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KEG2000-50A/B Elastomer
KEG2000-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KEG2000-75A/B Elastomer
KEG2000-75 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Shin-Etsu Silicones LIMSâ„¢ KEG2002-60A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
ASTM D955
Lubrizol Estane® S385A Thermoplastic Polyurethane
Type: Estane® S385A is a Shore 85A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
ASTM D955
Lubrizol Estane® S385AH Thermoplastic Polyurethane
Type: Estane® S385AH is a Shore 87A, polyester based thermoplastic polyurethane (TPU) with excellent transparency and Hydrolytic Stabilizer. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injectio..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
MD; ASTM D955
Aclo Accucomp Polyethylene HD0200L High Density
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Azoty Tarnow™ TARNOFORM 500 LS POM
High flow injection molding grade based on Tarnoform 500 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Azoty Tarnow™ TARNOFORM 500 POM
Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Azoty Tarnow™ TARNOFORM 700 POM
Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Diametrical Shrinkage
Asahi Glass Fluon® G340 PTFE Granular Powder
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Solvay Specialty Polymers Algoflon® A.30 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Solvay Specialty Polymers Algoflon® A.20 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner..
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
ASTM D955
PolyOne Synprene® IT38-004M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Choic..