Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.28 MPa | 330 psi | at 200%, as molded |
Multibase SILASTIC® C7-4550 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.28 MPa | 330 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.28 MPa | 330 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.28 MPa | 330 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 2.28 MPa | 330 psi | ASTM D412 |
Teknor Apex UNIPRENE® 2021 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 2.28 MPa | 330 psi | ASTM D412 |
Teknor Apex Uniprene® UN-2012-L3 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength, Yield | 2.28 MPa @Strain 300 % |
330 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT38-004M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Choic.. |
|||
Tensile Strength, Yield | >= 2.28 MPa | >= 331 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7045 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |