Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® IT 62-002 BLACK 2001 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® IT 62-002 BLACK 2001 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Over-Molding GradeUV StabilizedApplications: Multi-PurposeProcessing Method: Injection MoldingInformation provided by PolyOne Corporation
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ASTM D792
Linear Mold Shrinkage 0.017 cm/cm
0.017 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
10 Sec; ASTM D2240
64
64
Instant; ASTM D2240
Tensile Strength, Yield 4.76 MPa
690 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
3.17 MPa

@Strain 100 %
460 psi

@Strain 100 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
4.48 MPa

@Strain 300 %
650 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 430 %
430 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 20.7 kN/m
118 pli
Die C (graves), 20 in/min; ASTM D624