Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.990 g/cc | 0.990 g/cc | 23/23°C; ASTM D792 |
RheTech Products M12P250-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Filler panelsHVAC ductsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
LG Chemical NBR 6230 High Acrylonitrile Polymer Description: NBR 6230 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6230 is a non staining, low mooney, and m.. |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® DigiGuard® Gloss 110 Overprint varnish Description: Overprint varnish for flexible packagingUsage: DigiGuard® Gloss 110 is a high gloss, temperature resistant, water based overprint varnish which meets FDA food contact requirements.Ap.. |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® Licomer® W 485 Cationic montan emulsion Description: Cationic montan emulsionUsage: Licomer® W 485 is a high gloss emulsion that improves the performance of floor crystalllizers.Information provided by Michelman® |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® Michem® Emulsion 09625 Cationic ethylene acrylic acid emulsion Description: Cationic ethylene acrylic acid emulsionUsage: Michem® Emulsion 09625 provides excellent chemical resistance. Michem® Emulsion 09625 has proven most useful in floor and other polis.. |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® Michem® Emulsion 27720 Nonionic slip and anti-block additive Description: Nonionic slip and anti-block additiveUsage: Michem® Emulsion 27720 is a nonionic, amide emulsion used for anti-blocking, slip and mar resistant properties.We serve many markets throu.. |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® Michem® Emulsion 93335 Nonionic polyethylene emulsion Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93235 is a phenol free additive best used in water based coatings where improved slip, rub resistance, hardness and/or block res.. |
|||
Specific Gravity | 0.990 - 1.01 g/cc | 0.990 - 1.01 g/cc | |
Michelman® Michem® Flex P1831 Water based primer Description: Water based primer for liquids and extrusion coated resins.Usage: Michem® Flex P1831 is a primer for metal and paper substrates to promote adhesion to extrusion coated resins resulti.. |
|||
Specific Gravity | 0.990 - 1.02 g/cc | 0.990 - 1.02 g/cc | |
Michelman® Michem® Lube 160F Anionic carnauba wax emulsion Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160F provides superior slip and mar resistance on a variety of substrates such as metal, wood, film and paper. Anti-block properties .. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
LG Chemical NBR 6280 High Acrylonitrile Polymer Description: NBR 6280 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6280 is a non staining, high mooney, and .. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7190-1000 TPE Product Description: StarFlex P 7190-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
Teknor Apex Tekbond® TB 2007 Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Specific Gravity | 0.990 - 0.996 g/cc | 0.990 - 0.996 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2181HU High Flow, Fortified, Impact Resistant Polypropylene DescriptionPolyfort® FPP 2181HU is a high flow, fortified, impact resistant polypropylene, stabilized for UV resistance, and available in automotive matched colors. Information provided by A. Schul.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7673 COATING Syl-Off® 7673 Coating is a 100% active solids pre-catalysed, coating containing a medium viscosity vinyl endblocked only functional silicone polymer. Provides a particularly smooth, premium release.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | |
Dow Corning SYL-OFF® 7923 CATALYST EMULSION Syl-Off® 7923 Catalyst Emulsion is a 40% solids emulsion of vinyl functional polymer and platinum catalyst in water. A high performance catalyst recommended where fast cure speed is required.Inform.. |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® PMCP7010 Coating Syl-Off® 7010 Coating is a 100% active solids pre-catalysed, coating containing a low viscosity vinyl endblocked only functional silicone polymer. Provides a smooth, premium release performance and.. |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D1298 |
ExxonMobil 275 NC Mobiltac Mobiltac 375 NC, 325 NC and 275 NC extra high performance non-leaded, diluent-type, heavy-bodied open gear lubricants designed for a wide variety of open gear and mining applications. They contain a.. |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPMEM-1101 Emulsion Is chemically equivalent to DOW CORNING® 1101 EMULSION. Anionic, 50% active emulsion based on high viscosity polydimethylsiloxane.Information provided by Dow Corning |
|||
Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
Dow Corning 365 35% DIMETHICONE NF EMUSION White liquid emulsion containing 35% Dow Corning® 360 Medical Fluid, 350 cSt suitable for lubrication and siliconeization of glass, metals, plastics and rubber.Information provided by Dow Corning |
|||
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D471; ISO 2781 |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCHT Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040NCHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with
improved surface .. |