Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.7 kN/m | 118 pli | Die C; ASTM D624 |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Tear Strength | 20.7 kN/m | 118 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 62-002 BLACK 2001 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications: Multi-PurposeProcessing Method: Injection MoldingInformation provided by PolyOne Corporation |