Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Status: M6010SB meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows for, among other things, the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Certain limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Certain recommendations for processing M6010SB can only be made when the processing conditions, equipment and end use are provided; however, Equistar recommends that samples be produced and that users conduct their own testing in order to make their own independent determination that M6010SB is suitable and safe for their intended use and applications. Please contact your Equistar sales representative for more information.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 1.1 g/10 min
1.1 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 27.6 MPa
4000 psi
ASTM D882
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D882
Film Elongation at Break, MD 700 %
700 %
ASTM D882
Film Elongation at Break, TD 400 %
400 %
ASTM D882
Secant Modulus, MD 0.986 GPa
143 ksi
ASTM E111
Secant Modulus, TD 1.38 GPa
200 ksi
ASTM E111
Elmendorf Tear Strength MD 20 g
20 g
ASTM D1922
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Film Tensile Strength at Break, MD 60.7 MPa
8800 psi
ASTM D882
Film Tensile Strength at Break, TD 24.8 MPa
3600 psi
ASTM D882
Processing Properties Metric English Comments
Melt Temperature 199 - 210 °C
390 - 410 °F
Die Opening 0.1524 cm
0.06000 in
Blow-up Ratio (BUR) 2.2
2.2