Material Notes:
OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide polymers including PA6, PA6.6, PA11 and PA12. OnFlex™-S KA can be processed by 2K molding or overmolding, insert molding or co-extrusion. In addition to this, OnFlex™-S KA compounds are formulated to provide excellent compression set performance, even at elevated temperatures, a wide hardness range, good colourability and surface appearance, good mechanical properties and excellent UV resistance.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ISO 868
Tensile Strength at Break 7.50 MPa
1090 psi
ISO 37
Tensile Stress 3.90 MPa

@Strain 100 %
566 psi

@Strain 100 %
ISO 37
6.10 MPa

@Strain 300 %
885 psi

@Strain 300 %
ISO 37
Elongation at Break 500 %
500 %
ISO 37
Tear Strength 46.0 kN/m
262 pli
ISO 34-1
Compression Set 23 %

@Temperature 23.0 °C,
Time 259000 sec
23 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
38 %

@Temperature 70.0 °C,
Time 79200 sec
38 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
54 %

@Temperature 100 °C,
Time 79200 sec
54 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Melt Temperature 200 - 260 °C
392 - 500 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 100 °C
212 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Features Good Adhesion
Good UV Resistance
High Heat Resistance
Forms Pellets
Generic Material TPE
Generic Material Type Styrenic Thermoplastic Elastomer (TES)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Moderate
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Coextrusion
Multi Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications
Consumer Applications
Industrial Applications
Overmolding
Power/Other Tools