Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
PolyOne Maxxam™ FR MF5210-0301 DK GRAY 2451 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Network Polymers 779 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet) |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Techmer ES HiFill FR® HIPS 1000 FR-E Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Techmer ES HiFill FR® HIPS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Techmer ES HiFill FR® HIPS FR-1 Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 26.2 MPa | 3800 psi | ASTM D790 |
Ecomass® 4703ZD88 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym.. |