Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Paxon™ 7004 Crosslinkable Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Rotational Molding Grade
Manufacturer Exxon Chemical
Trade Name Paxon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Paxon™ 7004 Crosslinkable Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suited for applications that require excellent part fill during processing and outstanding finished part performance. Paxon™ 7000 series grades are all supplied with long term UV stabilization.Availability: Latin America, North America and South America Applications: Agricultural ProductsAutomotive ComponentsChemical Storage TanksLarge Refuse ContainersMarine Fuel TanksRecreational Vehicle – Fuel Tanks Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693A
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Modulus, 1% Secant 600 MPa
87000 psi
ASTM D790B
Izod Impact, Notched 2.30 J/cm

@Temperature -40.0 °C
4.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Impact Test 100 J

@Thickness 3.17 mm,
Temperature -40.0 °C
74.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
249 J

@Thickness 6.35 mm,
Temperature -40.0 °C
184 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
ASTM D638
Descriptive Properties Value Comments
Crosslink Potential 2.5
ExxonMobil Method