Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable W3204 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable W3204 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
15 sec; ASTM D2240
Tensile Strength 19.3 MPa

@Strain 100 %
2800 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Tensile Strength, Yield 23.4 MPa
3390 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 220 %
220 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
UL Temperature Rating
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Oxygen Index 26 %

@Thickness 3.18 mm
26 %

@Thickness 0.125 in
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1000 Hz
3.8

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 199 - 204 °C
390 - 399 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL 758
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 90%
113°C, 1.91 mm; 168 hr, UL Standard
Uses Wire & Cable Applications
Wire Types UL Style 1061