Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 19.3 MPa @Strain 100 % |
2800 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W3204 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength | 19.3 MPa | 2800 psi | ASTM D412 |
S&E Specialty Polymers GA-3133S-CCUV PVC Application: Meets style 1277 T.C. Power & Control Cable Requirements and can be used for CM(X), CATV(X) and CL2 jacketing applications. UL listed for 720hr. sunlightInformation provided by S&E Spec.. |
|||
Tensile Strength | 19.3 MPa | 2800 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-3188AHP PVC Compound Application: RoHS compliant, phthalate free, 105°C flame retardant jacketing material suitable for extrusion applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 19.3 MPa | 2800 psi | ASTM D638 |
Quadrant EPP TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet) |
|||
Tensile Strength | 19.3 MPa | 2800 psi | Optimum; With provided formulation; ASTM D638 |
PolyOne Geon™ 180 Series 180X5 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 180X5 is low molecular weight resin that provides good chemical foam characteristics with excellent overblow resistence. The modified rheology of Geon® 180X5 provides increased viscosity and.. |
|||
Tensile Strength | 19.3 MPa @Strain 100 % |
2800 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B6D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 19.3 MPa | 2800 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-1050 PVC Compound Application: A UL Bulletinized, VW-1, 105°C rated compound for THHN, THWN, MTW, 1000 volt applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 19.3 MPa | 2800 psi | Typical |
Garlock Super Rinohideâ„¢ 7160 SBR Rubber Lining SBR rubber lining for protection applications such as chute lining and skirtboards.Super RINOHIDEâ„¢, in particular, performs with superior resistance to abrasion, impact, aging and weathering. .. |
|||
Tensile Strength | 19.3 MPa | 2800 psi | Typical |
Garlock Viblonâ„¢ 266 Neoprene Bearing Pad Viblonâ„¢ pads are technically engineered and specifically designed to cushion impact, shock and vibration. Constructed of multiple layers of high-quality, cotton-polyester duck fabric, completel.. |
|||
Tensile Strength | 19.3 MPa | 2800 psi | ASTM D638 |
Ecomass® 4703BI74 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Tensile Strength | 19.3 MPa | 2800 psi | |
AlphaGary Garathane™ 6005 Polyurethane based compound A non-halogen, flame retardant, polyurethane compound for demanding cable jacket applications |
|||
Tensile Strength | 19.3 MPa | 2800 psi | ASTM D638 |
Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene Product CharacteristicsEasy processingGood impact resistanceESCRFood Contact CompliantUL Classification 94HBTypical ApplicationsCreamer and yot containersExtrusion/ thermoformingInformation provided.. |
|||
Tensile Strength | 19.3 MPa | 2800 psi | |
AlphaGary GW 2403-1 VW1 75 LCF Flame Retardant Polyvinyl Chloride 75°C rated jacket compound |
|||
Tensile Strength | 19.3 MPa | 2800 psi | 2 in/min; ASTM D638 |
Braskem TI6350WV High Impact Copolymer Polypropylene Description: Superior low temperature impact, nucleated, antistatic.Applications: Suggested uses include furniture, toys, compounding.Process: Injection Molding.This resin meets the requirements for.. |
|||
Tensile Strength | 19.3 MPa | 2800 psi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D4150 K (O/E SBS) Linear Triblock Copolymer Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton.. |