Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
15 sec; ASTM D2240
65
65
ASTM D2240
Tensile Strength at Break 6.89 MPa
999 psi
510 mm/min; ASTM D638
Tensile Strength 3.45 MPa

@Strain 100 %
500 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
510 mm/min; ASTM D638
Tear Strength 15.8 kN/m
90.2 pli
Die C, 510 mm/min; ASTM D624
Compression Set 30 %

@Temperature 23.0 °C,
Time 79200 sec
30 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 168 - 174 °C
334 - 345 °F
188 - 199 °C
370 - 390 °F
Descriptive Properties Value Comments
Features Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved