Material Notes:
Recommended for interior applications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
15 sec; ASTM D2240
90
90
ASTM D2240
Tensile Strength at Break 18.6 MPa
2700 psi
510 mm/min; ASTM D638
Tensile Strength 10.9 MPa

@Strain 100 %
1580 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 390 %
390 %
510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -33.9 °C
-29.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 5.0 %

@Thickness 1.91 mm
5.0 %

@Thickness 0.0750 in
ASTM D1003
Transmission, Visible 80 %

@Thickness 1.91 mm
80 %

@Thickness 0.0750 in
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Appearance Clear/Transparent
Features General Purpose
High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Film
General Purpose
Hose
Sheet
Tubing