Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0015 cm/cm
0.0010 - 0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 172 MPa
24900 psi
ASTM D790
Flexural Modulus 12.4 GPa
1800 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.44 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm - 1e+05
100 ohm-cm - 1e+05
ASTM D257
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 293 - 327 °C
559 - 621 °F
Mold Temperature 121 °C
250 °F
Drying Temperature 127 °C
261 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Features Flame Retardant
Filler / Reinforcement GlassCarbon Fiber Reinforcement
Forms Pellets
Generic Material PC
Generic Name Polycarbonate (PC)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America