Polymer Property : Tensile Modulus = 1800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.4 GPa
1800 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-NY-050-CU-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Modulus 12.4 GPa
1800 ksi
5 mm/min; ASTM D638
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Tensile Modulus 12.4 GPa
1800 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Tensile Modulus 12.4 GPa
1800 ksi
MTI ThermoStran® PA66-40G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Tensile Modulus 12.41 GPa
1800 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA (Asia Pacific)
LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Tensile Modulus 12.41 GPa
1800 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific)
LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret..
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Tensile Modulus 12.4 GPa
1800 ksi
1 mm/min
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
Tensile Modulus 12.4 GPa

@Treatment Temp. 70.0 °C,
Time 180000 sec
1800 ksi

@Treatment Temp. 158 °F,
Time 50.0 hour
62% rel. humidity
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..