Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen HP550K is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP550K is a homopolymer suitable for rope, tape, yarn, monofilament and sheet. Moplen HP550K resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Good mechanical propertiesApplications: Rope; Tape; Yarn; Monofilament; SheetInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Vicat Softening Point 154 °C
309 °F
ASTM D1525