Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.47 GPa | 213 ksi | |
Plastcom SLOVALEN PQ 83 T 20 PP, 20% mineral filling FeaturesModified PP for injection moulding with the content of 20% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Omni Plastics OmniTuff™ CPP TF20 Copolymer Polypropylene Talc Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP550K is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP550K is a homopolymer suitable for rope, tape, yarn, monofilament.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP552N Fiber (Staple) Grade Polypropylene Moplen HP552N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552N is a homopolymer selected by customers for use in high speed.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP552R Fiber (Staple/BCF/CF) Grade Polypropylene Moplen HP552R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552R is a homopolymer typically used by customers in high speed p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP553P Fiber (Staple) Grade Polypropylene Moplen HP553P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP553P is a homopolymer typically used by customers in high speed p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP562T Fiber (Spunbond) Grade Polypropylene Moplen HP562T is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562T is a homopolymer particularly suitable f.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP563S Fiber (Spunbond) Grade Polypropylene Moplen HP563S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP563S is a homopolymer typically used in spunb.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting & Profile Extrusion ResinCharacteristics: High Stiffness, Good Impact Resistance, Very Low Odor & Taste Transfer, Designated for Uniloy Blowmol.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene B200 PP B200 Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:StiffnessFormabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene B201Y PP B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene F400 PP F400 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene HJ340 PP HJ340 Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1% Secant; ASTM D790 |
Flint Hills P4C6Z-022 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene J742 PP J742 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporat.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene J945 PP J945 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D760 |
LG Chemical SEETEC H5300 Polypropylene, Homopolymer Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | |
Shinil Chemical SHINSTRA PP SE3501 Structural Polymer Bumper SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Flexural Modulus | 1.47 GPa @Thickness 3.20 mm |
213 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SH 2157 High Impact Polystyrene Characteristics Excellent ESCR properties Good formability Processing ExtrusionApplications Refrigerator door and cabinet liners Dairy containers Ice cream cups, plates and bowlsMaterial Status: .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6670B High Density Polyethylene Film Key Characteristics:High flowExcellent processabilityHigh stiffnessOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for drinking water, fruit juice, soft drink, milkI.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Braskem H 103 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling; food and cosmetic packing; toys and household; sealed closures. Information provided by Braskem |