Material Notes:
Moplen EP648N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP648N is a high gloss block copolymer particularly suitable for injection molding of parts of electrical appliances, containers. Moplen EP648N meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520.Features: Optimized balance of stiffness and toughness; High gloss; High stiffness; Heat resistance; Scratch resistance;Applications: Parts of electrical appliances; ContainersInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 9.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.81 GPa
263 ksi
ASTM D790
Izod Impact, Notched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648
Vicat Softening Point 153 °C
307 °F
ASTM D1525
Users viewing this material also viewed the following: