Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
PolyMirae Moplen RP210R Extrusion Coating and Lamination Grade Polypropylene Moplen RP210R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP210R is a copolymer particularly suitable for extrusion coating and.. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP513G30WBL Multi Reinforced PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Izod Impact, Notched | >= 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5100 PC/ABS+GF10% Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by.. |
|||
Izod Impact, Notched | 0.981 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUTENE-H ME2500 HDPE Description: LUTENE-H ME2500 is mainly intended for injection molding of bottle caps. It has good gas permeability characteristics and high toughness.Applications: Caps for beverage bottlesCAS No. 9.. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | |
Shinil Chemical SHINCON PES Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® T101G45 PET, 45% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2140 PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NT-7200 W ABS/PET, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1102 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NT-7200 W ABS/PET, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0813 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trihip® B500 High Impact Polystyrene Dimensional stability, electrical properties and weather resistance are excellent.B500 is the non-flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, P.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® D201G30 PBT, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-8102G MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | |
Zylog Hipolyene® 7151 M1 HF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
Cheng Yu Plastic ML849 Flame Retardant PC |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6GV30 Flame Retardant Nylon 6, 30% Glass Filled |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T883GV25 Flame Retardant PBT, 25% Glass Fiber |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® JN110 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G5F Nylon 66, 25% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G5 Nylon 66, 25% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | >= 0.981 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.84 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP2300 PP+GF30% Description: Injection Molding, PP+GF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® JN100 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |