Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded  (discontinued **)

Category Polymer , Thermoset , Phenolic
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive applications and can be molded by compression, transfer, or injection processes. Plenco drop ball 113g test value is 35 cm.Plenco has discontinued their Valite product line.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Water Absorption 0.35 %
0.35 %
ASTM D570
Linear Mold Shrinkage 0.0066 cm/cm
0.0066 in/in
Post shrinkage is 0.25% at 72hr 120°C.; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 91
91
ASTM D785
Tensile Strength, Ultimate 53.3 MPa
7730 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
Tensile Modulus 8.60 GPa
1250 ksi
ASTM D638
Flexural Yield Strength 81.8 MPa
11900 psi
ASTM D790
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Compressive Yield Strength 217.9 MPa
31600 psi
ASTM D695
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
J/cm; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 193 °C
379 °F
Heat Resistance; ASTM D795
Deflection Temperature at 1.8 MPa (264 psi) 183 °C
361 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.10 mm
V-0

@Thickness 0.240 in
Electrical Properties Metric English Comments
Electrical Resistivity 3.0725e+11 ohm-cm
3.0725e+11 ohm-cm
ASTM D257
Dielectric Constant 4.9

@Frequency 1e+6 Hz
4.9

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.5 kV/mm
292 kV/in
Short Term per ASTM D149.
Dissipation Factor 0.049

@Frequency 1e+6 Hz
0.049

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 140 sec
140 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved