Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4100 Phenolic, Granular, Injection Molded  (discontinued **)

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Heat Resistant Grade, Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4100 Phenolic, Granular, Injection Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and oil field applications and can be molded by compression, transfer, or injection.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Apparent Bulk Density 0.740 g/cc
0.0267 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.26 %
0.26 %
ASTM D570
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
per ATM D955. Post shrinkage is 0.26% at 72hr 120ºC per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 80
80
ASTM D785
Tensile Strength, Ultimate 57.4 MPa
8330 psi
ASTM D638
Elongation at Break 0.82 %
0.82 %
ASTM D638
Tensile Modulus 9.54 GPa
1380 ksi
ASTM D638
Flexural Yield Strength 89.8 MPa
13000 psi
ASTM D790
Flexural Modulus 8.44 GPa
1220 ksi
ASTM D790
Compressive Yield Strength 192.1 MPa
27860 psi
ASTM D695
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
ASTM D256
Impact 94
94
J/m Plenco drop ball test
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 201 °C
394 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 2.12e+11 ohm-cm
2.12e+11 ohm-cm
ASTM D257
Dielectric Constant 5.2

@Frequency 1e+6 Hz
5.2

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 7.40 kV/mm
188 kV/in
Step by Step; ASTM D149
10.9 kV/mm
277 kV/in
Short Time; ASTM D149
Dissipation Factor 0.066

@Frequency 1e+6 Hz
0.066

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 160 sec
160 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Users viewing this material also viewed the following: