Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | Radial shrinkage of 10 cm o.d. sintered rod at 23°C |
Solvay Specialty Polymers Algoflon® S 111 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | ASTM D955 |
PlastxWorld Veroplas PB2000 Nylon 66 general purpose, unfilled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | ASTM D955 |
PlastxWorld Veroplas PB2002 Nylon 66 impact modified, unfilled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | |
Azoty Tarnow™ TARNOFORM 400 LS POM Injection molding grade based on Tarnoform 400 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | |
Azoty Tarnow™ TARNOFORM 400 POM Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall detailsInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | Diametrical Shrinkage |
Asahi Glass Fluon® G307 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | |
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t.. |
|||
Linear Mold Shrinkage | 0.028 - 0.036 cm/cm | 0.028 - 0.036 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® 201-G0R PBT Resin Good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | Radial shrinkage of 10 cm o.d. sintered rod at 23°C |
Solvay Specialty Polymers Algoflon® F2 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | Diametrical Shrinkage |
Asahi Glass Fluon® G350 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |
|||
Linear Mold Shrinkage | 0.028 cm/cm | 0.028 in/in | ASTM D955 |
PlastxWorld Veroplas PB2009L Nylon 66 general purpose, unfilled, lubricated injection molding gradeInformation provided by PlastxWorld Inc. |