Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® B14E0 PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® B14E0 PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent flowability, high impact strength and toughness. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM 638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Yield Strength 79.3 MPa
11500 psi
ASTM D790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
0.25 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
0.25 inch; ASTM D648
Flammability, UL94 HB
HB