Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Flexural Yield Strength | 79.4 MPa | 11500 psi | DIN 53455; ASTM D790 |
Kolon SPESIN® KP513FLBL Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Flexural Yield Strength | 79.5 MPa | 11500 psi | ASTM D790 |
Plenco 7527 Phenolic, Nodular, Injection Molded
(discontinued **) Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco |
|||
Flexural Yield Strength | 79.4 MPa @Thickness 3.20 mm |
11500 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Yield Strength | 79.4 MPa @Thickness 3.20 mm |
11500 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 79.4 MPa @Thickness 3.20 mm |
11500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific) LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 79.4 MPa | 11500 psi | ASTM D790 |
Samyang Triloy® 220 Polymer Alloy, High Impact Excellent impact, formability and weather resistance.220 is a high impact grade.Applications: Automotive instrument panels and knob typesInformation provided by Samyang. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Electrablend® ABS SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackInformation pr.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® V3802 PBT + PC + PET (Asia Pacific) PBT + PC + PET, Mold Release, Flame retardant, Impact Modified, OpaqueThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific) This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
PlastxWorld CEVIAN® B14E0 PBT/ABS Alloy Excellent flowability, high impact strength and toughness. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
Chem Polymer Durlex 700 PBT, General Purpose A lubricated, general purpose PBT.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Flexural Yield Strength | 79.3 - 310 MPa @Temperature -40.0 - 150 °C |
11500 - 45000 psi @Temperature -40.0 - 302 °F |
Average value: 176 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Flexural Yield Strength | 79.4 MPa @Thickness 3.20 mm |
11500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR404T ABS, Heat Resistance Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical.. |