Plastics Group Polifil® 82MR Mineral-Reinforced Nylon 6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 82MR Mineral-Reinforced Nylon 6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in industrial clamp components as well as bearings. Standard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 5.17 GPa
750 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ASTM D648