Phillips 66 COPYLENE® CH003T Polypropylene, Homopolymer, Sheet

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CH003T Polypropylene, Homopolymer, Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
COPYLENE™ CH003T, a fractional melt flow polypropylene homopolymer resin, is available in pellet form. Replacement alternative for Pro-fax® HL561CInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.4 MPa
4700 psi
2 in/min; ASTM D638
Elongation at Yield 13.6 %
13.6 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Izod Impact, Notched 0.747 J/cm

@Temperature 23.0 °C
1.40 ft-lb/in

@Temperature 73.4 °F
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
unannealed; ASTM D648
Descriptive Properties Value Comments
Process Injection Molding