Polymer Property : Flexural Modulus = 10.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.9 GPa
1580 ksi
ASTM D790
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
Flexural Modulus 10.9 GPa
1580 ksi
(50.8 mm Span) 1mm/min; ASTM D790
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Flexural Modulus 10.9 GPa
1580 ksi
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
Flexural Modulus 10.9 GPa
1580 ksi
ASTM D790
Greene Tweed WRâ„¢ 300 PEEK, Carbon Filled
WR®300 is a carbon-fiber reinforced compression molded PEEK often selected by pump manufacturers and users for pump bushings and case or impeller wear rings. Maximum service life is achieved in ..
Flexural Modulus 10.9 GPa
1580 ksi
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Flexural Modulus 10.9 GPa
1580 ksi
ISO 178
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA), 25% GlassCarbon Fiber
Amodel® A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material..
Flexural Modulus 10.9 GPa
1580 ksi
ISO 178
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Flexural Modulus 10.9 GPa
1580 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DE0026E PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE0026E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 10.9 GPa
1580 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer
LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant.
Flexural Modulus 10.9 GPa
1580 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12
LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers.
Flexural Modulus 10.9 GPa
1580 ksi
ISO 178-93
Wellman Wellamid® GFX1717-BK1 Nylon 66, 43% Glass Fiber Reinforced, Silicone Lubricated
All information provided by Wellman Engineered Resins.
Flexural Modulus 10.9 GPa
1580 ksi
ASTM D790
A. Schulman ComAlloy Voloy® 684 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..
Flexural Modulus 10.9 GPa
1580 ksi
ISO 178
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material is ..
Flexural Modulus 10.9 GPa
1580 ksi
Phenolic 30%, Graphite fabric 70%
Phenyl silane - C.T.L "37-9X". Graphite fabric - "WCB"