Material Notes:
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Polymer Peyvand Co
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
ISO 527-2
Elongation at Break >= 10 %
>= 10 %
ISO 527-2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
Unannealed; ISO 75-2/C
Descriptive Properties Value Comments
Color Black