Material Notes:
Scotch® Heat Shrink Tubing FP-301VW has the same outstanding balance of electrical, physical and chemical properties as FP-301 tubing, and is specially engineered for excellent flame resistance. FP-301VW tubing is rated for continuous operation at -55°C to 135°C, and is designed to withstand elevated temperatures to 300°C for short periods. Minimum temperature for all FP-301VW tubing is 100°C.Information provided by 3M
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Water Absorption 0.20 %
0.20 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.5 MPa
2390 psi
Elongation at Break 400 %
400 %
175 %

@Temperature 175 °C,
Time 1.21e+6 sec
175 %

@Temperature 347 °F,
Time 336 hour
Heat Aged
2% Secant Modulus 0.0896 GPa
13.0 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
300 °C
572 °F
for short periods
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Strength 35.4 kV/mm
900 kV/in