Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive

Category Polymer , Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO FUSE SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications that require a relatively thick, viscous adhesive with flexible bondness. The fast curing qualities make it especially desirable in high speed industrial production. It is also ideal for applications on vertical or angled surfaces. Because of the 4000 viscosity, it works especially well in poor fitting applications such as rough metal or ceramic repair, unfinished metal to metal bonding, and metal to rubber. This product is a very good, thick, almost gel like adhesive.Part Numbers for this data: 04-190CF, 10-190CF, 15-190CF, 20-190CF, 25-190CF, 30-190CF, 35-190CFSoluble in Acetone, MEK, Amide, Methylene ChlorideInformation provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid State
Viscosity 3500 - 5000 cP
3500 - 5000 cP
Liquid State
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 90
80 - 90
Cured State
Tensile Strength 5.00 MPa
725 psi
Cured State
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Cured State
Softening Point 149 °C
300 °F
Cured State
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cured State
Flash Point 80.0 - 93.3 °C
176 - 200 °F
Liquid State
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.58e+14 ohm-cm
1.58e+14 ohm-cm
Dielectric Constant 2.44

@Frequency 1.00e+6 Hz
2.44

@Frequency 1.00e+6 Hz
Cured State
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Liquid State
Descriptive Properties Value Comments
Appearance Clear Liquid
Liquid State
Clear-Hard
Cured State
Base compound (Resin) Ethyl Cyanoacrylate
Liquid State
Gap Fill 0.009"
Cured State
Material Set Up Time <20 sec
Aluminum to Aluminum
<20 sec
Rubber to Rubber
10-20 sec
Polycarbonate to Polycarbonate
10-25 sec
Steel to Steel
30-50 sec
Phenolic to Phenolic