Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FC-0505-40All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 62
62
Tensile Strength, Ultimate 400 MPa
58000 psi
Tensile Strength, Yield 324 MPa
47000 psi
Elongation at Break <= 1.0 %
<= 1.0 %
Flexural Strength 703 MPa
102000 psi
Transverse Rupture
Bearing Yield Strength 0.000317 MPa
0.0460 psi
Charpy Impact, Unnotched 6.78 J
5.00 ft-lb