Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials F-200-P Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-10All information provided by Pacific Sintered Metals. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-216-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-216-P(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals Copper Steel FC-221-P Powdered Metal Medium strength mechanical components Equivalent MPIF Specification: FC-0205-35Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-200-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.00 - 6.40 g/cc | 0.217 - 0.231 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-200-P Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-10Information Provided by Pacific Sintered Metals, a division of PSM Industries |