Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 703 MPa | 102000 psi | Transverse Rupture |
Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Flexural Strength | 703 MPa | 102000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-200-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |