PTS Trilac® ABS-HH2350 High Heat ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer Polymer Technology & Services, LLC (PTS)
Trade Name Trilac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PTS Trilac® ABS-HH2350 High Heat ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 4.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 48.9 MPa
7090 psi
ASTM D638
Flexural Yield Strength 70.4 MPa
10200 psi
ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm

@Thickness 3.17 mm
2.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
237 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
ASTM D648
Flammability, UL94 HB

@Thickness 6.35 mm
HB

@Thickness 0.250 in