Oxford Polymers C-Acetal 25GF 25% Glass Fiber Reinforced Copolymer Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers C-Acetal 25GF 25% Glass Fiber Reinforced Copolymer Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
25% Glass Fiber Reinforced Copolymer AcetalInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Filler Content 25 %
25 %
Water Absorption 0.25 %
0.25 %
ASTM D570
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm

@Temperature 23.0 °C
10.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
ASTM D648