Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP) Information provided by PolyOne |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Oceanchem Group Potassium Formate 74-75% liquid Molecular Formula: KCOOHInformation Provided by Oceanchem Group |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Kuraray Genestarâ„¢ G1500A-M61 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. Main Features:High strengthHeat resistanceExamples of applications:Structural partsSteel alternating parts |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
KYDEX® 6200 LTR Thermoforming Sheet for Mass Transit Applications Features:Specifically designed for mass transit industriesCompliant with SMP800CMeets flamespread and smoke density requirements for mass transitExcellent formability and fabrication qualityGood def.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Sylvin Technologies 8999-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® AB9530 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 353 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 354 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Teknor Apex APEX® 65008 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Teknor Apex APEX® 96-A0914K-106 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 554 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Tufflake® 4615 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3000 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3000 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Mixed |
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrica.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Cheng Yu Plastic E2325 Flame Retardant PET, 25% Glass Fiber |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Dry; ASTM D792 |
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66 Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 530HTE NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate with Excellent High Temperature Dielectric PropertiesRynite 530HTE NC010 is a 30% glass reinforced modified polyethylene terephthalate resin with exce.. |