Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® 4114-14 GL (HS) , 14% Glass Fiber Reinforced, Impact Modified Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 4114-14 GL (HS) , 14% Glass Fiber Reinforced, Impact Modified Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nylene® 4114-14 GL (HS) is a 14% glass reinforced, high impact nylon 6/6. 4114-14 GL is automotive approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 78.6 MPa
11400 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 259 °C
498 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648