Material Notes:
Description: NGAC P907-30 is a high viscosity, controlled flow encapsulant designed for microelectronics applications requiring low shrinkage and high reliability performance.Advantages and Applications: Uses include protecting wire bonds and bare die and other micro-electronic structural assembly applications. NGAC P907-30 has a low CTE resulting in low shrinkage upon cure and no stress to substrates. It is highly resistant to humidity and will withstand reflow temperatures up to 260C.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Solids Content 100 %
100 %
Viscosity 300000 cP
300000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 95
95
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 1.00 min

@Temperature 150 °C
0.0167 hour

@Temperature 302 °F
2.00 min

@Temperature 120 °C
0.0333 hour

@Temperature 248 °F
300 min

@Temperature 100 °C
5.00 hour

@Temperature 212 °F
Pot Life 1440 min
1440 min
Descriptive Properties Value Comments
Color Black
Mix Ratio by Weight (R/H) 1/1/2009