Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NYCOA 2326 HS Super-Tough, Heat Stabilized Nylon 6 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer NYCOA, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 2326 HS Super-Tough, Heat Stabilized Nylon 6 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NYCOA 2326 HS is an impact modified, heat stabilized Nylon 6 resin, which offers outstanding toughness, impact strength and chemical resistance. NYCOA 2326 HS has been specially formulated to give a high degree of impact strength, without the loss of stiffness and rigidity. NYCOA 2326 HS processes easily on conventional injection molding and extrusion equipment. Typical applications include clips, fasteners, wiring harnesses, power tool housings, and connectors.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Water Absorption 1.7 %
1.7 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Flexural Strength 58.0 MPa
8410 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 8.75 J/cm
16.4 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648
Users viewing this material also viewed the following: