Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NEU NeuSoft™ 597-60A Industrial Ether TPU / SBC blend

Category Polymer , Thermoplastic , Polyurethane, TP , Silicone Polyurethane, Ether Based
Manufacturer NEU SPECIALTY ENGINEERED MATERIALS (PolyOne)
Trade Name NeuSoft™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NEU NeuSoft™ 597-60A Industrial Ether TPU / SBC blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.002 g/cc
0.03620 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength at Break 15.7 MPa
2280 psi
Tensile Stress 1.68 MPa

@Strain 100 %
244 psi

@Strain 100 %
5.58 MPa

@Strain 300 %
810 psi

@Strain 300 %
Elongation at Break 423 %
423 %
Tear Strength 40.1 kN/m
229 pli
Die C
Compression Set 19.7 %
19.7 %
Processing Properties Metric English Comments
Moisture Content <= 0.010 %
<= 0.010 %