Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.002 g/cc
0.03620 lb/in³
NEU NeuSoft™ 597-60A Industrial Ether TPU / SBC blend
Density 1.002 g/cc
0.03620 lb/in³
ISO 1183
Styrolution Styroflex® 2G 66 SBC
Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o..