International Mold Steel Daido DRM1 Matrix High-Speed Steel

Category Metal , Ferrous Metal , Tool Steel
Manufacturer International Mold Steel
Trade Name Daido
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF International Mold Steel Daido DRM1 Matrix High-Speed Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its higher toughness than conventional grade.Information provided by International Mold Steel
Mechanical Properties Metric English Comments
Hardness, Brinell <= 235
<= 235
Hardness, Rockwell C 56 - 58
56 - 58
40

@Treatment Temp. 700 °C
40

@Treatment Temp. 1290 °F
56

@Treatment Temp. 600 °C
56

@Treatment Temp. 1110 °F
59

@Treatment Temp. 520 °C
59

@Treatment Temp. 968 °F
Tensile Modulus 210 GPa
30500 ksi
Fatigue Strength 900 MPa

@# of Cycles 1.00e+7
131000 psi

@# of Cycles 1.00e+7
950 MPa

@# of Cycles 1.00e+6
138000 psi

@# of Cycles 1.00e+6
1000 MPa

@# of Cycles 100000
145000 psi

@# of Cycles 100000
Charpy Impact Unnotched 200 J/cm²
952 ft-lb/in²
59 HRC
260 J/cm²
1240 ft-lb/in²
57 HRC
Thermal Properties Metric English Comments
CTE, linear 11.2 µm/m-°C

@Temperature 20.0 - 100 °C
6.22 µin/in-°F

@Temperature 68.0 - 212 °F
11.7 µm/m-°C

@Temperature 20.0 - 300 °C
6.50 µin/in-°F

@Temperature 68.0 - 572 °F
12.2 µm/m-°C

@Temperature 20.0 - 500 °C
6.78 µin/in-°F

@Temperature 68.0 - 932 °F
12.7 µm/m-°C

@Temperature 20.0 - 700 °C
7.06 µin/in-°F

@Temperature 68.0 - 1290 °F
Specific Heat Capacity 0.413 J/g-°C

@Temperature 25.0 °C
0.0987 BTU/lb-°F

@Temperature 77.0 °F
0.519 J/g-°C

@Temperature 300 °C
0.124 BTU/lb-°F

@Temperature 572 °F
0.616 J/g-°C

@Temperature 500 °C
0.147 BTU/lb-°F

@Temperature 932 °F
0.840 J/g-°C

@Temperature 700 °C
0.201 BTU/lb-°F

@Temperature 1290 °F
Thermal Conductivity 22.4 W/m-K

@Temperature 25.0 °C
155 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
27.3 W/m-K

@Temperature 300 °C
189 BTU-in/hr-ft²-°F

@Temperature 572 °F
28.4 W/m-K

@Temperature 500 °C
197 BTU-in/hr-ft²-°F

@Temperature 932 °F
28.8 W/m-K

@Temperature 700 °C
200 BTU-in/hr-ft²-°F

@Temperature 1290 °F