Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 260 °C @Time 7.20e+7 sec |
500 °F @Time 20000 hour |
|
Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze The addition of 60% bronze to the base material reduces the expansion coefficient and gives lower sliding wear.Special Properties:• Lower sliding wear than Murflor®• Good slide properties• Low s.. |
|||
Maximum Service Temperature, Air | 260 °C @Time 7.20e+7 sec |
500 °F @Time 20000 hour |
|
Murtfeldt Murflor® Polytetrafluoroethylene Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with.. |
|||
Maximum Service Temperature, Air | 260 °C @Time 7.20e+7 sec |
500 °F @Time 20000 hour |
|
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon The integration of 25% carbon increases the wear resistance, hardness, and creep strength of this material. Murflor® + Carbon is used, for example, when electrical conductivity is required and Mate.. |
|||
Maximum Service Temperature, Air | 260 °C @Time <=86400 sec |
500 °F @Time <=24.0 hour |
|
Murtfeldt Murinit® SP Polyphenylene Sulfide Thanks to the low fiber content and integrated solid lubricant, Murinit® SP offers an excellent combination of good slide and wear behavior, high strength, and dimensional stability – even at high.. |