Material Notes:
Mineral filled PP concentrate formulated to meet resin furniture properties at 1:1 dilution with polypropylene. The product contains UV and TiO2 adequate to stabilize the total product.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792-91
Melt Flow 18 g/10 min
18 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.6 MPa
2700 psi
ASTM D638-95
Elongation at Break 300 %
300 %
ASTM D638-95
Flexural Strength 35.9 MPa
5210 psi
ASTM D790-95
Flexural Modulus 2.586 GPa
375.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256-93a