Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.9 MPa | 5210 psi | ASTM D790-95 |
Multibase Multi-Pro® 4005 M I Medium Impact 40% Filler Content Polypropylene Multi-Pro 4005 M I is a chemically coupled reinforced polypropylene compound featuring high flex modulus and high impact under retention of the heat resistance properties. The product is designed f.. |
|||
Flexural Strength | 35.9 MPa | 5210 psi | ASTM D790 |
PolyOne Maxxam™ PPH-20C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 35.9 MPa | 5210 psi | ASTM D790 |
PolyOne Maxxam™ PPH-20C UV Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled Information provided by Niche Polymer |
|||
Flexural Strength | 35.9 MPa | 5210 psi | ASTM D790 |
Niche Polymer PPCT40BK Copolymer PP, 40% Talc Filled Information provided by Niche Polymer |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
I. Stern BLK100 High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetProfilesAgency Rating.. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® HDPE 0226 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0096 S LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0096 S2 LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0096 S3 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0112 B AM2 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Antimicrobial (Fungicide)Information provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0121 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0202 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0254 S Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0254 S1 003 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® HIPS TM10 WT155 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® HIPS TM40 WT 40% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 40% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® PP 0112 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES Luriblend® HIPS TL10 BK Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Good Wear Resistance, Low Friction and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall Appliances.. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Americas Styrenics STYRON® 484 High Impact Polystyrene Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliances/RefrigerationPackaging/disposablesHousewaresInformation pr.. |
|||
Flexural Strength | 35.9 MPa | 5200 psi | ASTM D790 |
Techmer ES HiFill® HIPS 0212 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |