Solvay ALKAMULS® 504/V Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® 504/V Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: ETHYLENE GLYCOL DISTEARATECAS: 627-83-8Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Ethylene glycol distearate is widely used in cosmetics as pearlizing or opacifying agent. When properly formulated in shampoo, bodywash, hand soaps or other liquid soaps it will form a crystalline structure that gives a pearlescent appearance. Typical use level is 0.5 to 3%. In creams and lotions it will provide opacity and some emoliency. Alkamuls 504V is provided in a solid flake form which must be heated in the available water portion of the formula to approximately 70-75C. Pearlescence will occur upon cooling. For liquid pearlescent systems see Rhodia’s Mirasheen product line.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Thermal Properties Metric English Comments
Melting Point 70.0 - 75.0 °C
158 - 167 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Descriptive Properties Value Comments
Appearance Clear, pale yellow-green liquid
Molten, RP-0064
White to pale yellow flake
RP-0064
Composition Diester
>92%, RP-1407
Ethylene Glycol
<0.5%, RP-1407
Fatty Acid
<0.1%, RP-1407
Monoester
<8.0%, RP-1407