Multibase Multi-Pro® 2513 C Whirlpool White Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 2513 C Whirlpool White Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 24.1 MPa
3500 psi
ASTM D790
Flexural Modulus 1.03 GPa
150 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
73°F; ASTM D256
Gardner Impact 22.60 J
16.67 ft-lb
ASTM D3029
Optical Properties Metric English Comments
Gloss 35 %
35 %
at 60°; ASTM D2457