Multibase Multi-Flex® TPO D 5308-20 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D 5308-20 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass reinforced TOP with improved stiffness and retention of low temperature resistance.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792-91
Melt Flow 7.0 g/10 min
7.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate >= 20.69 MPa
>= 3001 psi
ASTM D638-95
Elongation at Break >= 18 %
>= 18 %
ASTM D638-95
Flexural Strength 24.8 MPa
3600 psi
ASTM D955-89
Flexural Modulus >= 1.586 GPa
>= 230.0 ksi
Secant 1%; ASTM D-790-95
Gardner Impact 4.90 J
3.61 ft-lb
ASTM D5420-93